Next Article in Journal
Impact and Post-Impact Performance of Sandwich Wall Boards with GFRP Face Sheets and a Web-Foam Core: The Effects of Impact Location
Next Article in Special Issue
Structure and Electron Mobility of ScN Films Grown on α-Al2O3(1102) Substrates
Previous Article in Journal
Impact of Two-Dimensional Particle Size Distribution on Estimation of Water Vapor Diffusivity in Micrometric Size Cellulose Particles
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Investigating Metal–Insulator Transition and Structural Phase Transformation in the (010)-VO2/(001)-YSZ Epitaxial Thin Films

1
School of Electronic Science and Applied Physics, Hefei University of Technology, Hefei 230009, China
2
National Synchrotron Radiation Laboratory, University of Science and Technology of China, Hefei 230026, China
3
School of Physics and Electronic Information, Henan Polytechnic University, Jiaozuo 454000, China
*
Authors to whom correspondence should be addressed.
Materials 2018, 11(9), 1713; https://doi.org/10.3390/ma11091713
Submission received: 18 August 2018 / Revised: 5 September 2018 / Accepted: 11 September 2018 / Published: 13 September 2018
(This article belongs to the Special Issue Advances in Epitaxial Materials)

Abstract

:
The VO2 thin films with sharp metal–insulator transition (MIT) were epitaxially grown on (001)-oriented Yttria-stabilized zirconia substrates (YSZ) using radio-frequency (RF) magnetron sputtering techniques. The MIT and structural phase transition (SPT) were comprehensively investigated under in situ temperature conditions. The amplitude of MIT is in the order of magnitude of 104, and critical temperature is 342 K during the heating cycle. It is interesting that both electron concentration and mobility are changed by two orders of magnitude across the MIT. This research is distinctively different from previous studies, which found that the electron concentration solely contributes to the amplitude of the MIT, although the electron mobility does not. Analysis of the SPT showed that the (010)-VO2/(001)-YSZ epitaxial thin film presents a special multi-domain structure, which is probably due to the symmetry matching and lattice mismatch between the VO2 and YSZ substrate. The VO2 film experiences the SPT from the M1 phase at low temperature to a rutile phase at a high temperature. Moreover, the SPT occurs at the same critical temperature as that of the MIT. This work may shed light on a new MIT behavior and may potentially pave the way for preparing high-quality VO2 thin films on cost-effective YSZ substrates for photoelectronic applications.

1. Introduction

Vanadium dioxide (VO2), which is a typical strongly correlated transition metal oxide, exhibits a first-order metal–insulator transition (MIT) [1,2], which is usually accompanied by a structural phase transition (SPT) from a low-temperature monoclinic semiconductor to a high-temperature rutile metal with a hysteresis of a few kelvins [3]. VO2 has the advantages of both reversible and sharp electronic resistivity and optical transmittance changes in the vicinity of MIT (~340 K, near room temperature), which happens in response to different external stimuli, including photons, temperature, electric field, magnetic field, electrical chemistry, and stress [4,5,6,7]. Due to these properties, VO2 can be potentially used as a material in numerous applications in electronic and optical devices, such as memory devices [4], Mott field effect transistors [5], thermochromic smart windows [6], and so on.
VO2 thin-film structures on the various substrates are still important for the applications in solid-state electronic and optical devices [8,9]. Moreover, the MIT properties can be modulated by substrate engineering; for example, through the proper choice of substrate orientation [10], pre-treatment of the substrate surface [11,12], selection of a substrate type with different lattice parameters [8,13], and so on. Yang et al. observed the anisotropic MIT in the selected (110)-oriented VO2/TiO2 thin films [10]. Liu et al. used a focused-ion-beam patterning TiO2 substrates to control phase separation in the VO2 thin films [12]. Then Lee et al. selected the SrTiO3, LaAlO3 substrates to stabilize the VO2 polymorphs [13]. Therefore, significant effort has been exerted into ensuring the successful growth of high-quality VO2 epitaxial thin films on certain substrates, such as LaAlO3, TbScO3, Al2O3, MgAl2O4, SrTiO3, YSZ, TiO2, and so on [8,10,11,14,15,16]. Ramanathan examined the growth of M1 phase VO2 thin films on complex oxide single-crystal substrates ((111)-LaAlO3, (0001)-Al2O3, (111)-MgAl2O4, (111)-MgO) with 3m surface symmetry using RF sputtering techniques [8]. After this, Venkatesan et al. grew high-quality M1 VO2 thin films on a SrTiO3 substrate by controlling the vanadium arrival rate and oxidation of the V atoms using pulse laser deposition techniques [15]. After those, Lee et al. comprehensively investigated the epitaxial stabilization of M1 VO2 on the perovskite-oxide substrates, including TbScO3, SrTiO3, (LaAlO3)0.3(SrAl0.5Ta0.5O3)0.7, and LaAlO3 using pulsed laser epitaxy [13]. Recently, Lee et al. reported that the polymorphic (010)-VO2(M1) grew epitaxially on the cubic (001)-YSZ substrate [14]. However, they did not carefully study the MIT behaviors and the SPT in the (010)-VO2/(001)-YSZ thin films. So far, there has been a lack of comprehensive investigation into both the MIT and structural phase transformation in this system. On the other hand, from the viewpoint of the engineering applications of the VO2 thin films, the wafer-scale YSZ with good optical transmittance is a more cost-effective substrate compared to perovskite oxide single crystals [8,14]. Therefore, combined with the advances made in the RF sputtering techniques, the high-quality VO2/YSZ epitaxial thin films in the wafer-scale size may be an attractive candidate material for photoelectronic applications in the future [9,17,18].
Motivated by the above-mentioned progress in the thin-film heterostructures based on VO2 and the lack of research on the MIT and the SPT in the new VO2/YSZ thin films, we utilized the RF sputtering techniques to grow high-quality (010)-VO2/(001)-YSZ thin films in this present study. The MIT behaviors and the SPT were comprehensively studied. The four orders of magnitude of the MIT were achieved, which resulted from the coactions of electron concentration and mobility. The SPT happens synchronously with the occurrence of the MIT. This work potentially provides a way to prepare wafer-scale VO2/YSZ thin films and also gives a new insight into the MIT in this system.

2. Materials and Methods

2.1. Film Fabrication

A RF sputtering technique was employed for growing epitaxial VO2 thin film on (001)-oriented Yttria-stabilized zirconia (YSZ, Zr:Y ratio approximately 91:9) substrates. One-side-polished YSZ crystals were commercially bought from MTI Corp. (Hefei, China). A vanadium metal disk of 99.99% purity with a diameter of 2 inches was used as the sputtering target and was water-cooled during deposition. The base pressure of the system was 2.8 × 10−4 Pa. The substrate temperature was set to 550 °C. The gas-flow rates of the pure Ar and O2 were set to 39 and 8 standard cubic centimeters per minute, respectively. The total pressure for film growth was approximately 0.52 Pa. The sputtering power was chosen as 60 W. The thickness of the VO2 thin film in this work was approximately 90 nm and was achieved by controlling the deposition time, which was reported in our previous results [19,20,21].

2.2. Structural Characterizations

X-ray diffraction (XRD, Rigaku, Tokyo, Japan) and Raman spectroscopy were employed to investigate microstructural properties. The θ–2θ scans were collected on the X-ray diffractometer with the temperature being varied in situ (Rigaku Smart-lab, Tokyo, Japan, Cu Kα ~ 1.5406 Å). Due to the weak intensity of the asymmetric diffraction peaks, the Φ scans were carried out on the beamline 14B in Shanghai synchrotron radiation facilities (SSRF, Shanghai, China) at room temperature in order to determine the domain structures and epitaxial relationship in the VO2 thin films. Raman spectroscopy with an acquisition time of 1 s was conducted using the XploRATM Raman spectrometer (HORIBA Scientific, Ltd., Paris, France) with in situ controlling temperature across the MIT. A 532-nm laser of 0.25 mW was used as the excitation source with a 100× microscope objective. Each Raman spectrum was repeated three times until the temperature in situ was stable.

2.3. Transport Property Measurements

The transport properties were measured on the Hall-effect measurement system (HMS-5500, Ecopia, Korea) using the van der Pauw method. The four Au/Ti (200 nm/20 nm) electrodes were deposited by electron beam evaporation at room temperature. The four probes of the Hall-effect measurement system pressed on the electrodes for the transport measurements.

3. Results and Discussion

3.1. Phase and Domain Structures in the VO2/YSZ Thin Films

A wide-angle θ–2θ scan of the VO2/YSZ thin films was performed at room temperature. The corresponding results are shown in Figure 1a. First, the Bragg’s angles at 39.8° and 85.7° correspond to the (020) and (040) peaks of the VO2 thin films, respectively, which are the feature diffraction peaks for the M1 phase of VO2 [14,18,22]. The YSZ (001) and (002) peaks are also marked in Figure 1a. The absence of any other peaks of the VO2 thin films in the XRD pattern indicates that no other phases of vanadium oxide are present. Hence, the pure M1 VO2 thin films were successfully grown on the (001)-YSZ substrate using an RF magnetron sputtering technique. Second, the VO2 thin films are highly oriented along the out-of-plane direction with the (010) planes parallel to the (001) surface of the YSZ substrates, which is namely [ 010 ] V O 2 // [ 001 ] YSZ .
To obtain information about the epitaxial relationship of the VO2 film with respect to the YSZ substrate, Φ scans were performed on the YSZ (113) and VO2 (011) peaks. The four YSZ (113) peaks with the 90° separation are seen in Figure 1b and are marked using solid lines. This fourfold symmetry is definitely ascribed to the nature of the cubic symmetry of the YSZ substrate [14]. Figure 1c shows the Φ scan of the VO2 (011) peaks. There are 12 peaks, which are divided into three types of domain structures, which are namely Domain 1 (deep blue dots), Domain 2 (light blue dots), and Domain 3 (red dots), which is shown in Figure 1c. Every domain has four VO2 (011) peaks, which are all located at an angle of 90° from each other. This is another of saying that the VO2 (011) peaks show fourfold symmetry in the Φ scan. However, it is well-known that the M1 VO2 (P21/c space group) must show twofold symmetry in the Φ scan along the rotating axis of [010] direction [23]. It is reasonable that Domain 1 has two different configurations, which has been supported by the findings of Zou and Lee [14,24]. Figure 1d presents the two types of configurations of Domain 1, which are referred to as Domain 1A and 1B. The dashed and dotted lines in Figure 1d show the projected directions of the YSZ (113) and VO2 (022) planes projected directions on the surface of the substrates. The two projected directions have an intersection angle of 45°, which is consistent with the Φ scans shown in Figure 1b,c. Hence, the in-plane epitaxial relationship is [ 100 ] V O 2 // [ 010 ] YSZ in the domain 1A or [ 100 ] YSZ in the Domain 1B. The configurations of Domain 2 and 3 are sketched in the Figures S1 and S2, respectively. The observed domain structure of the (010)-VO2/(001)-YSZ epitaxial thin film is quite distinctive compared to the cases in the epitaxial thin film systems of VO2/Al2O3 [24], VO2/SrTiO3 [25], and VO2/TiO2 [20]. The multi-domain structures in the VO2/YSZ epitaxial thin films are due to the lattice mismatch and surface symmetry match between VO2 and the YSZ substrate [14]. This fundamental question will be comprehensively investigated in the future. This striking domain structure may play an important role in the MIT in the VO2/YSZ epitaxial thin films.

3.2. Studies of Metal–Insulator Transitions

The MIT behaviors were characterized by obtaining the transport properties measurement using the van der Pauw method, which is shown in Figure 2a. The resistivity is a function of heating temperature, as shown in Figure 2b. At 301 and 379 K, the resistivity is 11.1 × 10−4 and 9.3 × 10−4 Ω·cm, respectively. As a consequence, the amplitude of resistivity change is approximately 1.2 × 104 at the low and high temperature, as shown in Figure 2b. This amplitude of MIT is comparable with the cases of the VO2/Al2O3 and VO2/TiO2 epitaxial thin films [21,26]. Additionally, the temperature of MIT is about 342 K in the heating cycle, which is consistent with the temperature of 340 K for the bulk VO2 [27]. It is known that the VO2 is an n-type semiconductor in the insulating phase (M1). After the resistivity measurements, the electron concentration and mobility were also measured using the van der Pauw method (please see the detailed procedures in Section 2 of the Supplementary Materials). Both are roughly increased by the order of magnitude of 102 across the MIT, which is shown in Figure 2c,d. It is mentionable that the beating of the mobility and concentration data is due to the displacement of the four probes, resulting from the magnet mechanical movements during measurements (please see Figure S3 in the Supplementary Materials). Therefore, the amplitude of the MIT is about 104, since the resistivity is positively proportional to the product of the electron concentration and mobility. The change in the electron concentration was the sole contribution to the amplitude of the MIT, both in the VO2 single crystals [28] and VO2/Al2O3 thin film system [29]. However, in this work, both electron concentration and mobility contribute to the MIT in the VO2/YSZ system. This important and interesting observation may encourage the further studies of the MIT mechanism, which may be quite different from the cases in the other VO2 film systems. For the mechanisms of this observation, on one hand, the unique domain structure may contribute to the co-actions of the mobility and carrier concentration to the MIT [19]. On the other hand, the oxygen vacancy and defect may play a prominent role in the mobility and carrier concentration across the MIT [30,31]. The detailed studies on these two mechanism are underway and will be present elsewhere.

3.3. Investigating Structural Phase Transitions

Since the SPT often accompanies the MIT [32], the microstructural characterizations were performed using Raman spectroscopy and high-resolution XRD under variable temperature conditions in situ. Figure 3a,b show the Raman spectra during the heating and cooling process. First, the feature Raman peaks at the wavenumbers 192, 223, and 614 cm−1 are clearly observed, which were ascribed to the Ag modes of the VO2 labelled by the stars in Figure 3. This result indicates the phase type of M1 VO2. This result is also fairly consistent with the aforementioned XRD patterns. Second, in the heating cycle, the feature Raman peaks disappear at 343 K in Figure 3a, indicating an occurrence of SPT from M1 to the R phase [33]. The SPT temperature is close to that of MIT (~342 K), as determined by transport measurements in Section 3.2. During the cooling process, the feature Raman peaks appear at 338 K, which implies a phase transition from the metallic rutile phase to the insulating M1 phase. The thermal hysteresis (about 5 K) shows a typical first-order phase transition in the (010)-VO2/(001)-YSZ epitaxial thin films, which is quite similar to the results of the VO2/Al2O3 [33], VO2/TiO2 (including the (110)-, (100)-, and (101)-VO2/TiO2 thin films, whether the thickness thin or thick) [10,20], and VO2/SrTiO3 thin films [25].
To further elucidate the SPT across the MIT, the local XRD θ–2θ scans were collected with variable temperatures in situ. In Figure 4a, the (020) peak is shifted down from 39.779° at 303 K to 39.638° at 373 K. Thus, the distance of (020) planes is increased from the low-temperature M1 phase to the high-temperature R phase. To more clearly show the SPT, numerous local θ–2θ scans in the heating and cooling cycles were obtained, which are shown in Figure 4b,c. The sharp shifts of (020) peaks are marked by dashed lines in Figure 4b,c. The SPT temperatures are approximately 343 K and 338 K during the heating and cooling process, respectively. These results are consistent with the transport property measurements and Raman spectra. To quantitatively study the SPT, the lattice constant b was measured. First, as increasing and decreasing temperature, the θ–2θ scans of (020) peaks of the VO2 thin film were obtained. The b-axis is just perpendicular to this characteristic (020) plane. Hence the spacing of the (020) planes directly reflects the lattice constant b. Second, the position (2θ) of the (020) peaks can be read out from the θ–2θ scans curves as patterned in Figure 4b,c. Third, using Bragg formula b·sin(2θ/2) = λ, the lattice constant b can be easily calculated. Consequently, the lattice constant b (defined in the notion of monoclinic symmetry) is plotted in Figure 4d. The marked feature was a sharp increase in the lattice constant b from 4.529 Å at the low temperature to 4.545 Å at the high temperature, evidencing the occurrence of SPT at 340 K [34]. Therefore, the occurrence of SPT is a natural concomitant of the MIT in the (010)-VO2/(001)-YSZ film system. This behavior was also found in the M1 VO2/Al2O3 thin films [31], but was different from the case in the thinner (001)-VO2/TiO2 film system. In the thinner case, the SPT is suppressed by epitaxial strain, although the MIT continues in the (001)-VO2/TiO2 thin films [20].

4. Conclusions

In summary, the high-quality M1 (010)-VO2 thin films were grown epitaxially on the cubic (001)-YSZ substrates. Both the MIT and structural phase transformation were studied. First, the amplitude of the MIT in the VO2/YSZ thin films is in the order of magnitude of 104, while the MIT temperature is about 342 K during the heating process. Second, the co-actions of electron concentration and mobility on the MIT in this VO2 film system are different from the cases seen in the other system. This result may be due to the distinctive domain structures of the monoclinic VO2 thin films on the cubic YSZ substrates. Third, the SPT transforms from the low-temperature M1 phase to the high-temperature rutile phase during the heating process, which was determined by Raman spectroscopy and high-resolution XRD. The temperature of the SPT is nearly same as that of the MIT. Hence, when the VO2/YSZ thin films experience the MIT, the SPT will occurs synchronously. This work may highlight another novel VO2 thin-film system, which probably has a novel MIT mechanism. Our findings may pave the way to using these thin films on cost-effective substrates in photoelectronic applications.

Supplementary Materials

The following are available online at https://www.mdpi.com/1996-1944/11/9/1713/s1, Figure S1: Domain configurations of Domain 2; Figure S2: Domain configurations of Domain 3, Figure S3: (a) Ecopia HMS-5000 Hall Measurement System. (b) The four-probe stage with movable magnets.

Author Contributions

Y.Y. (Yuanjun Yang) and Z.L. conceived the idea of this work. Y.Y. (Yuanjun Yang) and Y.Y. (Yingxue Yao) wrote this paper. B.Z. plotted the figures. H.L. collected data of this paper. C.G. helped design the experiments and acquired the funding. C.Z. and C.K. fabricated the samples and analyzed the data. All the authors revised and finally approved the paper.

Funding

This study was partially supported by the National Key Research Program of China (2016YF0300102). This work at Hefei University of Technology was mainly funded by the Fundamental Research Funds for the Central Universities (108-4115100092). It was also partially supported by the Natural Science Foundation of China (51402281, 11775224, U1532142, and 11504358).

Acknowledgments

The authors are particularly grateful for the beamtime from the beamline (14B) of Shanghai Synchrotron Radiation Facilities and for help from Yueliang Gu, Guangzhi Yin, Xingmin Zhang, Tieying Yang, and Xingyu Gao in the XRD characterizations and analysis.

Conflicts of Interest

The authors declare no conflict of interest. The funders had no role in the design of the study; in the collection, analyses, or interpretation of data; in the writing of the manuscript, or in the decision to publish the results.

References

  1. Brahlek, M.; Zhang, L.; Lapano, J.; Zhang, H.T.; Engel-Herbert, R.; Shukla, N.; Datta, S.; Paik, H.; Schlom, D.G. Opportunities in vanadium-based strongly correlated electron systems. MRS Commun. 2017, 7, 27–52. [Google Scholar] [CrossRef]
  2. Quackenbush, N.F.; Paik, H.; Woicik, J.C.; Arena, D.A.; Schlom, D.G.; Piper, L.F.J. X-Ray spectroscopy of ultra-thin oxide/oxide heteroepitaxial films: A case study of single-nanometer VO2/TiO2. Materials 2015, 8, 5452–5466. [Google Scholar] [CrossRef] [PubMed]
  3. Chen, Y.L.; Wang, Z.W.; Chen, S.; Ren, H.; Wang, L.X.; Zhang, G.B.; Lu, Y.L.; Jiang, J.; Zou, C.W.; Luo, Y. Non-catalytic hydrogenation of VO2 in acid solution. Nat. Commun. 2018, 9, 818. [Google Scholar] [CrossRef] [PubMed]
  4. Driscoll, T.; Kim, H.T.; Chae, B.G.; Kim, B.J.; Lee, Y.W.; Jokerst, N.M.; Palit, S.; Smith, D.R.; Di Ventra, M.; Basov, D.N. Memory metamaterials. Science 2009, 325, 1518–1521. [Google Scholar] [CrossRef] [PubMed]
  5. Nakano, M.; Shibuya, K.; Okuyama, D.; Hatano, T.; Ono, S.; Kawasaki, M.; Iwasa, Y.; Tokura, Y. Collective bulk carrier delocalization driven by electrostatic surface charge accumulation. Nature 2012, 487, 459–462. [Google Scholar] [CrossRef] [PubMed]
  6. Ke, Y.; Zhou, C.; Zhou, Y.; Wang, S.; Chan, S.H.; Long, Y. Emerging thermal-responsive materials and integrated techniques targeting the energy-efficient smart window application. Adv. Funct. Mater. 2018, 28, 1800113. [Google Scholar] [CrossRef]
  7. Ke, Y.; Wang, S.; Liu, G.; Li, M.; White, T.J.; Long, Y. Vanadium dioxide: The multistimuli responsive material and its applications. Small 2018, 1802025. [Google Scholar] [CrossRef] [PubMed]
  8. Wongn, F.J.; Zhou, Y.; Ramanathan, S. Epitaxial variants of VO2 thin films on complex oxide single crystal substrates with 3m surface symmetry. J. Cryst. Growth 2013, 364, 74–80. [Google Scholar] [CrossRef]
  9. Hong, B.; Zhao, J.; Hu, K.; Yang, Y.; Luo, Z.; Li, X.; Gao, C. Facile synthesis of various epitaxial and textured polymorphs of vanadium oxide thin films on the (0006)-surface of sapphire substrates. RSC Adv. 2017, 7, 22341–22346. [Google Scholar] [CrossRef] [Green Version]
  10. Hu, K.; Yang, Y.; Hong, B.; Zhao, J.; Luo, Z.; Li, X.; Zhang, X.; Gu, Y.; Gao, X.; Gao, C. Thickness-dependent anisotropy of metal–insulator transition in (110)-VO2/TiO2 epitaxial thin films. J. Alloys Compd. 2017, 699, 575–580. [Google Scholar] [CrossRef]
  11. Yang, Y.; Wang, L.; Huang, H.; Kang, C.; Zong, H.; Zou, C.; Lu, Y.; Li, X.; Hong, B.; Gao, C. Controlling metal–insulator transition in (010)-VO2/(0001)-Al2O3 epitaxial thin film through surface morphological engineering. Ceram. Int. 2018, 4, 3348–3355. [Google Scholar] [CrossRef]
  12. Corder, S.N.G.; Jiang, J.; Chen, X.; Kittiwatanakul, S.; Tung, I.-C.; Zhu, Y.; Zhang, J.; Bechtel, H.A.; Martin, M.C.; Lawrence Carr, G.; et al. Controlling phase separation in vanadium dioxide thin films via substrate engineering. Phys. Rev. B 2017, 96, 161110. [Google Scholar] [CrossRef]
  13. Lee, S.; Ivanov, I.N.; Keum, J.K.; Lee, H.N. Epitaxial stabilization and phase instability of VO2 polymorphs. Sci. Rep. 2016, 6, 19621. [Google Scholar] [CrossRef] [PubMed]
  14. Choi, S.; Chang, S.J.; Oh, J.; Jang, J.H.; Lee, S. Electrical and optical properties of VO2 polymorphic films grown epitaxially on Y-stabilized ZrO2. Adv. Electron. Mater. 2018, 4, 1700620. [Google Scholar] [CrossRef]
  15. Srivastava, A.; Rotella, H.; Saha, S.; Pal, B.; Kalon, G.; Mathew, S.; Motapothula, M.; Dykas, M.; Yang, P.; Okunishi, E.; et al. Selective growth of single phase VO2(A, B, and M) polymorph thin films. APL Mater. 2015, 3, 026101. [Google Scholar] [CrossRef]
  16. Hong, B.; Yang, Y.; Hu, K.; Yang, M.; Luo, Z.; Li, X.; Gao, C. Dynamic strain control of the metal–insulator transition and non-volatile resistance switching in (010) VO2/(111) Pb(Mg1/3Nb2/3)0.7Ti0.3O3 epitaxial heterostructures. Mater. Lett. 2017, 196, 108–111. [Google Scholar] [CrossRef]
  17. Wu, J.M.; Chang, W.E. Ultrahigh responsivity and external quantum efficiency of an ultraviolet-light photodetector based on a single vo2 microwire. ACS Appl. Mater. Interfaces 2014, 6, 14286–14292. [Google Scholar] [CrossRef] [PubMed]
  18. Zhang, H.T.; Zhang, L.; Mukherjee, D.; Zheng, Y.X.; Haislmaier, R.C.; Alem, N.; Engel-Herbert, R. Wafer-scale growth of VO2 thin films using a combinatorial approach. Nat. Commun. 2015, 6, 8475. [Google Scholar] [CrossRef] [PubMed]
  19. Hong, B.; Hu, K.; Tao, Z.; Zhao, J.; Pan, N.; Wang, X.; Lu, M.; Yang, Y.; Luo, Z.; Gao, C. Polymorph separation induced by angle-distortion and electron delocalization effect via orbital modification in VO2 epitaxial thin film. Phys. Rev. B 2017, 95, 075433. [Google Scholar] [CrossRef]
  20. Yang, M.; Yang, Y.; Hong, B.; Wang, L.; Hu, K.; Dong, Y.; Xu, H.; Huang, H.; Zhao, J.; Chen, H.; et al. Suppression of structural phase transition in VO2 by epitaxial strain in vicinity of metal–insulator transition. Sci. Rep. 2016, 6, 23119. [Google Scholar] [CrossRef] [PubMed]
  21. Yang, M.; Yang, Y.; Hong, B.; Wang, L.; Luo, Z.; Li, X.; Kang, C.; Li, M.; Zong, H.; Gao, C. Surface-growth-mode-induced strain effects on the metal–insulator transition in epitaxial vanadium dioxide thin films. RSC Adv. 2015, 5, 80122–80128. [Google Scholar] [CrossRef]
  22. Yang, M.; Yang, Y.; Hong, B.; Huang, H.; Hu, S.; Dong, Y.; Wang, H.; He, H.; Zhao, J.; Liu, X.; et al. Resistance switching of epitaxial VO2/Al2O3 heterostructure at room temperature induced by organic liquids. AIP Adv. 2015, 5, 037114. [Google Scholar] [CrossRef]
  23. Zhao, Y.; Lee, J.H.; Zhu, Y.; Nazari, M.; Chen, C.; Wang, H.; Bernussi, A.; Holtz, M.; Fan, Z. Structural, electrical, and terahertz transmission properties of VO2 thin films grown on c-, r-, and m-plane sapphire substrates. J. Appl. Phys. 2012, 111, 053533. [Google Scholar] [CrossRef]
  24. Fan, L.L.; Wu, Y.F.; Si, C.; Pan, G.Q.; Zou, C.W. Synchrotron radiation study of VO2 crystal film epitaxial growth on sapphire substrate with intrinsic multi-domains. Appl. Phys. Lett. 2013, 102, 011604. [Google Scholar] [CrossRef]
  25. Wang, L.; Yang, Y.; Zhao, J.; Hong, B.; Hu, K.; Peng, J.; Zhang, H.; Wen, X.; Luo, Z.; Li, X.; et al. Growth temperature-dependent metal–insulator transition of vanadium dioxide epitaxial films on perovskite strontium titanate (111) single crystals. J. Appl. Phys. 2016, 119, 145301. [Google Scholar] [CrossRef]
  26. Aetukuri, N.B.; Gray, A.X.; Drouard, M.; Cossale, M.; Gao, L.; Reid, A.H.; Kukreja, R.; Ohldag, H.; Jenkins, C.A.; Arenholz, E.; et al. Control of the metal–insulator transition in vanadium dioxide by modifying orbital occupancy. Nat. Phys. 2013, 9, 661–666. [Google Scholar] [CrossRef]
  27. Fisher, B.; Patlagan, L. Switching VO2 single crystals and related phenomena: Sliding domains and crack formation. Materials 2017, 10, 554. [Google Scholar] [CrossRef] [PubMed]
  28. Hosevear, W.H.; Paul, W. Hall Effect in VO2 near the semiconductor-to-metal transition. Phys. Rev. B 1973, 7, 2109–2111. [Google Scholar] [CrossRef]
  29. Ruzmetov, D.; Heiman, D.; Claflin, B.B.; Narayanamurti, V.; Ramanathan, S. Hall carrier density and magnetoresistance measurements in thin-film vanadium dioxide across the metal–insulator transition. Phys. Rev. B 2009, 79, 153107. [Google Scholar] [CrossRef]
  30. Faber, H.; Das, S.; Lin, Y.H.; Pliatsikas, N.; Zhao, K.; Kehagias, T.; Dimitrakopulos, G.; Amassian, A.; Patsalas, P.A.; Anthopoulos, T.D. Heterojunction oxide thin-film transistors with unprecedented electron mobility grown from solution. Sci. Adv. 2017, 3, e1602640. [Google Scholar] [CrossRef] [PubMed]
  31. Zhang, Z.; Zuo, F.; Wan, C.; Dutta, A.; Kim, J.; Rensberg, J.; Nawrodt, R.; Park, H.H.; Larrabee, T.J.; Guan, X.F.; et al. Evolution of metallicity in vanadium dioxide by creation of oxygen vacancies. Phys. Rev. Appl. 2017, 7, 034008. [Google Scholar] [CrossRef]
  32. Park, J.H.; Coy, J.M.; Serkan Kasirga, T.; Huang, C.M.; Fei, Z.Y.; Hunter, C.; Cobden, D.H. Measurement of a solid-state triple point at the metal–insulator transition in VO2. Nature 2013, 500, 431–444. [Google Scholar] [CrossRef] [PubMed]
  33. Ji, Y.; Zhang, Y.; Gao, M.; Yuan, Z.; Xia, Y.; Jin, C.; Tao, B.; Chen, C.; Jia, Q.; Lin, Y. Role of microstructures on the M1-M2 phase transition in epitaxial VO2 thin films. Sci. Rep. 2014, 4, 4854. [Google Scholar] [CrossRef] [PubMed]
  34. McGee, R.; Goswami, A.; Pal, S.; Schofield, K.; Bukhari, S.A.M.; Thundat, T. Sharpness and intensity modulation of the metal–insulator transition in ultrathin VO2 films by interfacial structure manipulation. Phys. Rev. Mater. 2018, 2, 034605. [Google Scholar] [CrossRef]
Figure 1. (a) XRD θ–2θ scans for the (010)-VO2/(001)-YSZ thin films; (b) The Φ scan of the substrate YSZ (113) peaks; (c) The Φ scan of the VO2 (011) peaks; (d) The schematic of the domain structures of the VO2 epitaxial thin film on the YSZ substrate.
Figure 1. (a) XRD θ–2θ scans for the (010)-VO2/(001)-YSZ thin films; (b) The Φ scan of the substrate YSZ (113) peaks; (c) The Φ scan of the VO2 (011) peaks; (d) The schematic of the domain structures of the VO2 epitaxial thin film on the YSZ substrate.
Materials 11 01713 g001
Figure 2. Metal–insulator transition characterizations. (a) The schematic of the transport measurement using the van der Pauw method; (b) the resistivity vs. temperature curve; (c) the electron mobility and (d) concentration as temperature increases.
Figure 2. Metal–insulator transition characterizations. (a) The schematic of the transport measurement using the van der Pauw method; (b) the resistivity vs. temperature curve; (c) the electron mobility and (d) concentration as temperature increases.
Materials 11 01713 g002
Figure 3. Raman spectra in the cases of increasing (a) and decreasing (b) temperature. The stars labelled in the figure represent the Ag modes in the VO2 thin films. The shade boxes show the Raman signals from the YSZ substrates.
Figure 3. Raman spectra in the cases of increasing (a) and decreasing (b) temperature. The stars labelled in the figure represent the Ag modes in the VO2 thin films. The shade boxes show the Raman signals from the YSZ substrates.
Materials 11 01713 g003
Figure 4. The structural phase transition studied by XRD. (a) The local XRD θ–2θ scans of the VO2 (020) peaks at 303 and 373 K. The evolutions of the VO2 (020) peaks under increasing (b) and decreasing (c) temperatures. (d) The lattice constant b vs. the temperature curve.
Figure 4. The structural phase transition studied by XRD. (a) The local XRD θ–2θ scans of the VO2 (020) peaks at 303 and 373 K. The evolutions of the VO2 (020) peaks under increasing (b) and decreasing (c) temperatures. (d) The lattice constant b vs. the temperature curve.
Materials 11 01713 g004

Share and Cite

MDPI and ACS Style

Yang, Y.; Yao, Y.; Zhang, B.; Lin, H.; Luo, Z.; Gao, C.; Zhang, C.; Kang, C. Investigating Metal–Insulator Transition and Structural Phase Transformation in the (010)-VO2/(001)-YSZ Epitaxial Thin Films. Materials 2018, 11, 1713. https://doi.org/10.3390/ma11091713

AMA Style

Yang Y, Yao Y, Zhang B, Lin H, Luo Z, Gao C, Zhang C, Kang C. Investigating Metal–Insulator Transition and Structural Phase Transformation in the (010)-VO2/(001)-YSZ Epitaxial Thin Films. Materials. 2018; 11(9):1713. https://doi.org/10.3390/ma11091713

Chicago/Turabian Style

Yang, Yuanjun, Yingxue Yao, Benjian Zhang, Hui Lin, Zhenlin Luo, Chen Gao, Cong Zhang, and Chaoyang Kang. 2018. "Investigating Metal–Insulator Transition and Structural Phase Transformation in the (010)-VO2/(001)-YSZ Epitaxial Thin Films" Materials 11, no. 9: 1713. https://doi.org/10.3390/ma11091713

APA Style

Yang, Y., Yao, Y., Zhang, B., Lin, H., Luo, Z., Gao, C., Zhang, C., & Kang, C. (2018). Investigating Metal–Insulator Transition and Structural Phase Transformation in the (010)-VO2/(001)-YSZ Epitaxial Thin Films. Materials, 11(9), 1713. https://doi.org/10.3390/ma11091713

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop