Next Issue
Volume 1, December
Previous Issue
Volume 1, June
 
 

Chemosensors, Volume 1, Issue 2 (September 2013) – 1 article , Pages 3-20

  • Issues are regarded as officially published after their release is announced to the table of contents alert mailing list.
  • You may sign up for e-mail alerts to receive table of contents of newly released issues.
  • PDF is the official format for papers published in both, html and pdf forms. To view the papers in pdf format, click on the "PDF Full-text" link, and use the free Adobe Reader to open them.
Order results
Result details
Section
Select all
Export citation of selected articles as:
878 KiB  
Review
Autonomous Oscillation of Nonthermoresponsive Polymers and Gels Induced by the Belousov–Zhabotinsky Reaction
by Yusuke Hara
Chemosensors 2013, 1(2), 3-20; https://doi.org/10.3390/chemosensors1020003 - 11 Sep 2013
Cited by 5 | Viewed by 9519
Abstract
This review introduces the self-oscillating behavior of two types of nonthermoresponsive polymer systems with Ru catalyst moieties for the Belousov-Zhabotinsky (BZ) reaction: one with a poly-vinylpyrrolidone (PVP) main chain, and the other with a poly(2-propenamide) (polyacrylamide) (PAM) main chain. The amplitude of the [...] Read more.
This review introduces the self-oscillating behavior of two types of nonthermoresponsive polymer systems with Ru catalyst moieties for the Belousov-Zhabotinsky (BZ) reaction: one with a poly-vinylpyrrolidone (PVP) main chain, and the other with a poly(2-propenamide) (polyacrylamide) (PAM) main chain. The amplitude of the VP-based self-oscillating polymer chain and the activation energy for self-oscillation are hardly affected by the initial concentrations of the BZ substrates. The influences of the initial concentrations of the BZ substrates and the temperature on the period of the swelling-deswelling self-oscillation are examined in detail. Logarithmic plots of the period against the initial concentration of one BZ substrate, when the concentrations of the other two BZ substrates are fixed, show good linear relationships. The period of the swelling-deswelling self-oscillation decreases with increasing temperature, in accordance with the Arrhenius equation. The maximum frequency (0.5 Hz) of the poly(VP-co-Ru(bpy)3) gel is 20 times that of the poly(NIPAAm-co-Ru(bpy)3) gel. It is also demonstrated that the amplitude of the volume self-oscillation for the gel has a tradeoff with the self-oscillation period. In addition, this review reports the self-oscillating behavior of an AM-based self-oscillating polymer chain as compared to that of the VP-based polymer chain. Full article
(This article belongs to the Special Issue Hydrogel-Based Chemosensors)